Applying 3M 5200 in cold weather
Moderators: a j r, TDockside, Miles, Moderators
Applying 3M 5200 in cold weather
I am refastening my 1960 Seacoaster below the waterline which involves (among other things) removing the machine screws, prying the laps (or is it the strakes?) apart, applying 3M 5200, then putting in new machine screws. My works space is unheated although I have a propane space heater to take the edge off when I'm working. Living in New Hampshire it gets a bit cool this time of year and I am concerned that the 5200 won't cure properly. I can apply the 5200 above the recommended 40 degree but once the propane heater is shut off it cools down pretty quickly and stays cold until I fire the heater back up.
I really want to be able to get this part of the job done over the next month or two but don't want to mess things up. Does anyone have any thoughts?
Thanks for your help.
Paul
I really want to be able to get this part of the job done over the next month or two but don't want to mess things up. Does anyone have any thoughts?
Thanks for your help.
Paul
Life is too short to own an ugly boat
What do the instructions for the material tell you? I am betting the 3M5200 must have a minimum temperature. That means not just the air around the boat but the wood of the boat itself and for the alloted time period the material needs for curing.
If the container does not tell you, give 3M a call.
Andreas
If the container does not tell you, give 3M a call.
Andreas
I also need to re-seal the planks below the waterline in my Seacoaster so I did a search on that product right after reading your post. A lot of people advise staying away from that product unless you want the repair to be Permanent! Some recommend Sika-flex instead and also advise to stay away from a silicone product at all costs.
Verne
Verne
The 3M 5200 is $25.00 per 10oz tube. The Sikaflex 221 is $6.25 per 10oz tube. How many tubes will it take to do your lapstrake? Try a Google on the Sikaflex product. Compare the specs on tensile strength, tear resistance, shear resistance, movement, elongation and shrink. Sikaflex can also be sanded and painted.
Just trying to help........... (I have no connection to either company)
Verne
Just trying to help........... (I have no connection to either company)
Verne
-
- Posts: 106
- Joined: Wed Jul 19, 2006 6:59 pm
- Location: Vernon, WI
I had the very same question and called the 877 number on the tube for Marine Technical Support. I was told that there would be no problem if the work area dropped in temperature below the recommended application temperature. In fact, the temp can drop below freezing. The curing process will take longer as it does not cure in extreme cold. However, the curing process picks up again with warmer temps. The main caution is that the 5200 MUST cure before you can paint over it. How do you know it is cured? If you push on it, it should feel like firm rubber. If it is "squishy", it's not yet cured. Hope this helps.
-
- Posts: 106
- Joined: Wed Jul 19, 2006 6:59 pm
- Location: Vernon, WI
That's good to know. I can get the temp of the boat up by placing some incandescent light under the upturned hull. I figure if I keep them burning when I'm not using the heater I can at least keep the hull wood at around 40 degrees. I'm not sure how much of the 5200 I'll need to buy but the container indicates a small bead, which is what I'll require should get me between 30 and 100 linear feet.
For what it is worth, Jamestown Distributors has the 10 oz tube of 3M 5200 for 12.99, plus shipping.
Paul
For what it is worth, Jamestown Distributors has the 10 oz tube of 3M 5200 for 12.99, plus shipping.
Paul
Life is too short to own an ugly boat